  • Article
    Citation - WoS: 11
    Citation - Scopus: 13
    On the Detailed Mechanical Response Investigation of PHBV/PCL and PHBV/PLGA Electrospun Mats
    (IOP Publishing Ltd, 2019-03-29) Bal, Burak; Tugluca, Ibrahim Burkay; Koc, Nuray; Isoglu, Ismail Alper
    In this study, electrospun mats of pristine poly(epsilon-caprolactone) (PCL), Poly(D, L-lactide-co-glycolide) (PLGA), poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV), as well as PHBV/PCL blends and PHBV/PLGA blends in different ratios (80:20, 75:25, 50:50, 25:75, 20:80, 10:90, 5:95%, w/w) and Centella Asiatica (CA) loaded (1, 5, 10%, w/v) PHBV/PCL and PHBV/PLGA polyester blends were prepared. Electrospun mats were characterized by scanning electron microscopy (SEM) in order to show uniform and bead and defect-free fiber structure with average diameter. The blend ratio and strain rate dependencies of mechanical behavior of these electrospun membranes were investigated under tensile loading. The tensile tests were conducted at an initial strain rates of 10(-1) s(-1), 10(-2) s(-1), 10(-3) s(-1) and 10(-4) s(-1) at room temperature and the best and worst combinations of PHBV/PLGA, PHBV/PCL blend ratios for both stress and ductility required applications were specified for each strain rate. The effects of blend ratios on the tensile strength and Young's modulus were also investigated. Moreover, the effects of Centella Asiatica on the electrospun membranes' mechanical behavior were demonstrated at different strain rates. Consequently, this study constitutes an important guideline for the selection and usage of the aforementioned electrospun membranes as a wound dressing material in terms of mechanical response at different loading scenarios.
  • Article
    Citation - WoS: 22
    Citation - Scopus: 28
    High-Concentration Carbon Assists Plasticity-Driven Hydrogen Embrittlement in a Fe-High Mn Steel With a Relatively High Stacking Fault Energy
    (Elsevier Science SA, 2018-02) Tugluca, Ibrahim Burkay; Koyama, Motomichi; Bal, Burak; Canadinc, Demircan; Akiyama, Eiji; Tsuzaki, Kaneaki
    We investigated the effects of electrochemical hydrogen charging on the mechanical properties of a Fe-33Mn-1.1C austenitic steel with high carbon concentration and relatively high stacking fault energy. Hydrogen pre charging increased the yield strength and degraded the elongation and work-hardening capability. The increase in yield strength is a result of the solution hardening of hydrogen. A reduction in the cross-sectional area by subcrack formation is the primary factor causing reduction in work-hardening ability. Fracture modes were detected to be both intergranular and transgranular regionally. Neither intergranular nor transgranular cracking modes are related to deformation twinning or simple decohesion in contrast to conventional Fe-Mn-C twinning induced plasticity steels. The hydrogen-assisted crack initiation and subsequent propagation are attributed to plasticity-dominated mechanisms associated with strain localization. The occurrence of dynamic strain aging by the high carbon content and ease of cross slip owing to the high stacking fault energy can cause strain/damage localization, which assists hydrogen embrittlement associated with the hydrogen-enhanced localized plasticity mechanism.
  • Article
    Citation - WoS: 105
    Citation - Scopus: 114
    Effect of Strain Rate on Hydrogen Embrittlement Susceptibility of Twinning-Induced Plasticity Steel Pre-Charged With High-Pressure Hydrogen Gas
    (Pergamon-Elsevier Science Ltd, 2016-09) Bal, B.; Koyama, M.; Gerstein, G.; Maier, H. J.; Tsuzaki, K.
    The effects of tensile strain rate on the hydrogen-induced mechanical and microstructural features of a twinning-induced plasticity (TWIP) steel were investigated using a Fe-23Mn-0.5C steel with a saturated amount of hydrogen. To obtain a homogeneous hydrogen distribution, high-pressure hydrogen gas pre-charging was performed at 423 K. Similar to previous studies on hydrogen embrittlement, the deterioration in the tensile properties became distinct when the strain rate was decreased from 0.6 x 10(-3) to 0.6 x 10(-4) s(-1). In terms of microstructural features, hydrogen-precharging decreased the thickness of deformation twin plates, and it localized dislocation slip. Moreover, facets of the hydrogen induced quasi-cleavage feature on the fracture surface became smoother with decreasing strain rate. In this study, we proposed that a combined effect of hydrogen segregation, slip localization, and thinning of twin plates causes the hydrogen embrittlement of TWIP steels, particularly at a low strain rate. (C) 2016 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.