Production of Mn3O4 Nanoparticles From a Manganiferous Iron Ore via Reductive Leaching, Precipitation, and Calcination

No Thumbnail Available

Date

2022

Journal Title

Journal ISSN

Volume Title

Publisher

Elsevier

Open Access Color

Green Open Access

No

OpenAIRE Downloads

OpenAIRE Views

Publicly Funded

No
Impulse
Top 10%
Influence
Average
Popularity
Top 10%

Research Projects

Journal Issue

Abstract

The synthesis of Mn3O4 nanoparticles from a manganiferous iron ore through reductive leaching, precipitation, and calcination was investigated. The reductive leaching results showed that Mn (99.9%) was almost completely extracted into the leaching solution along with a substantial amount of Mg (99.9%), Al (99.5%), Ca (80%), and Fe (22.9%) under the following conditions: 30 g/L tartaric acid as a reducing agent, 1 M HCl solution, leaching temperature of 90 ?, and leaching duration of 3 h. In the first precipitation step, Fe and Al were expelled from the pregnant leach solution by the addition of NaOH prior to conducting the precipitation experiments for the production of manganese carbonate (MnCO3) particles from the purified solution. In the second precipitation step, MnCO3 particles were produced using sodium carbonate (Na2CO3) as the precipitating agent. The effects of parameters such as reaction temperature, Na2CO3 concentration, and experimental duration were investigated using the Taguchi approach. Manganse(II) was precipitated in the form of MnCO3 particles (97.4%) under the following conditions: a temperature of 30 ?C, Na2CO3 concentration of 0.014 mol/L, and duration of 30 min. The precipitate was observed to have a structure similar to that of rhodochrosite (MnCO3). Thermogravimetric/ differential thermal analyses were subsequently performed in three different atmospheres (air, oxygen, and nitrogen) to select a suitable atmosphere for calcination. The experimental results indicated the formation of hausmannite (Mn3O4) with a purity of 97.5% Mn3O4, 0.42% MgO, 1.66% CaO, and 0.34% FeO. The specific surface area, particle size, Curie temperature, magnetisation, coercivity, and remanence ratio of the final product obtained via 3 h of calcination at 350 C were estimated to be 133.3 m(2)/g, < 142.2 nm, 56 K, 10.10 Am-2/kg, 0.35 T, and 0.19, respectively. The characterisation results revealed the excellent low-temperature ferromagnetic properties of the produced Mn3O4 nanoparticles.

Description

Kursunoglu, Sait/0000-0002-1680-5482; Top, Soner/0000-0003-3486-4184

Keywords

Manganiferous Iron Ore, Mn3O4 Nanoparticles, Reductive Leaching, Precipitation, Calcination

Turkish CoHE Thesis Center URL

Fields of Science

02 engineering and technology, 0210 nano-technology, 01 natural sciences, 0104 chemical sciences

Citation

WoS Q

Q1

Scopus Q

Q1
OpenCitations Logo
OpenCitations Citation Count
6

Source

Hydrometallurgy

Volume

208

Issue

Start Page

105810

End Page

PlumX Metrics
Citations

CrossRef : 7

Scopus : 9

Captures

Mendeley Readers : 8

SCOPUS™ Citations

10

checked on Feb 03, 2026

Web of Science™ Citations

8

checked on Feb 03, 2026

Page Views

7

checked on Feb 03, 2026

Google Scholar Logo
Google Scholar™
OpenAlex Logo
OpenAlex FWCI
0.70329906
Altmetrics Badge

Sustainable Development Goals

SDG data is not available