Scopus İndeksli Yayınlar Koleksiyonu

Permanent URI for this collectionhttps://hdl.handle.net/20.500.12573/395

Browse

Search Results

Now showing 1 - 3 of 3
  • Article
    Citation - Scopus: 2
    Zeolite Synthesis by Alkali Fusion Method Using Two Different Fly Ashes Derived From Turkish Thermal Power Plants
    (Chamber of Mining Engineers of Turkey, 2020-03-01) Top, S.; Vapur, Hüseyin
    In this study, Faujasite (Na-LSX) (3.5(Ca0.3)3.5(Na0.6)3.5(Mg0.1)Al7Si17O48 32(H2O)) type zeolites and Ca-Filipsite (CaK0.6Na0.4Si5.2Al2.8O16 6(H2O)) type zeolites were produced from Sugözü Thermal Power Plant and Çatalaǧzi Thermal Power Plant fly ashes by alkali fusion method followed by water leaching, respectively. In these methods, fly ashes and sodium hydroxide (NaOH) were mixed in certain proportions and sintered at 600°C in ash furnace. Then, zeolites were obtained from the ground materials after water leaching and solid/liquid separation, respectively. Cation Exchange Capacity (CEC), X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Fourier-Transform Infrared Spectroscopy (FTIR), X-Ray Fluorescence (XRF) and Atomic Absorption Spectrometer (AAS) analyses were used to characterize the synthesized zeolites. The zeolites synthesized with Sugözü fly ashes in a ratio of 1:2 had 136.93 meq/100 g CEC, whereas the CEC of synthesized zeolite from Çatalaǧzi fly ashes was found to be 247.88 meq/100 g. As a result, zeolites, which can be used as wastewater treatment agent, energy storage material, catalyst and separator, were synthesized by using 2 different Class F fly ash. © 2023 Elsevier B.V., All rights reserved.
  • Article
    Citation - Scopus: 17
    Hydrometallurgical Processing of Nickel Laterites- A Brief Overview on the Use of Solvent Extraction and Nickel/Cobalt Project for the Separation and Purification of Nickel and Cobalt;
    (Chamber of Mining Engineers of Turkey, 2019-06-01) Kursunoglu, Sait; Kaya, Muammer
    In this study, a brief overview of the solvent extraction (SX) application for the separation and purification of nickel and cobalt in hydrometallurgical processing of laterite nickel ores is presented. This paper consists of two parts: firstly, the SX of nickel and cobalt from sulphate leach solutions is described; and secondly, the development of hydrometallurgical plants for the processing of laterite nickel ores that involve solvent extraction technique is discussed. The most important extractants are shortly given in the first part of the study. It is seen that the extraction and separation of nickel and cobalt from the impure leach solution of laterite nickel ores can be performed by either using a single extractant system that is called as a direct solvent extraction (DSX) or a mixture of two or more extractant which is known as a synergistic solvent extraction system (SSX). Mixed sulphide precipitation (MSP) and mixed hydroxide precipitation (MHP) processes are mentioned. This paper is also addressed advantage and disadvantages of each extraction system. It is shown that capital investment expenditure, operational investment expenditure and mineralogical content are the most important factors that can affect the selection of the appropriate hydrometallurgical process for lateritic nickel ore. © 2023 Elsevier B.V., All rights reserved.
  • Article
    Citation - Scopus: 6
    Extraction of Lanthanum and Cerıum from a Bastnasite Ore By Direct Acidic Leaching
    (Chamber of Mining Engineers of Turkey, 2020-06-01) Kursunoglu, Sait; Top, S.; Hussaini, Shokrullah; Gokcen, H. S.; Altiner, Mahmut; Ozsarac, Safak; Kaya, Muammer
    The extraction of lanthanum (La) and cerium (Ce) from a bastnasite ore by direct acidic leaching was investigated. The effects of acid concentration and leaching temperature on the extraction of La and Ce from the ore were tested. Using nitric (NHO3), more than 85% of the La and Ce were simultaneously extracted into leach solution whereas the La and Ce dissolutions were determined as less than 85% by using sulfuric acid (H2SO4). The La dissolution exceeded 90% by using hydrochloric acid (HCl); however, the Ce dissolution remained below 85% under the following conditions: solid-to-liquid ratio of 20% (w/v), the acid concentration of 20%, leaching temperature of 25°C and leaching time of 1 h. The result revealed that HNO3 could be used as a solvent for the maximum simultaneous extraction of the La and Ce from the bastnasite ore. The leaching temperature had no crucial effect on the dissolution of La and Ce when HNO3 or HCl solutions were preferred as a solvating agent. However, the leaching temperature had a slight positive effect on the dissolutions of La and Ce when H2SO4 was used as a solvent. © 2023 Elsevier B.V., All rights reserved.