    Recovery of Lithium From Spent Coin-Type Lithium Manganese Dioxide Cr Cells by Acidic Leaching in the Presence of Potassium Permanganate as Oxidant
    (Springer, 2022-09-20) Kursunoglu, Sait; Top, Soner; Altiner, Mahmut; Ozsarac, Safak; Kaya, Muammer
    The selective leaching of lithium from spent coin-type lithium manganese dioxide CR cells by oxidative leaching and precipitation of Li2CO3 from Li-bearing leach solution has been experimentally and theoretically investigated. The oxidative leaching experiments were carried out using sulfuric acid in the presence of potassium permanganate (KMnO4). The dissolutions of lithium, manganese, nickel, and cobalt were found to be 84.8%, 0.9%, 46.6%, and 9.7%, respectively. The results demonstrated that a considerable amount of manganese and cobalt remained in the leach residue. The Li-bearing leach solution was fed to an impurity removal stage. It was observed that a substantial amount of lithium loss, along with manganese, nickel, and cobalt, was determined at pH 10. At standard temperature and pressure, the species of lithium as a function of pH, lithium concentration, and carbonate concentration was evaluated for the generation of Li2CO3 from the oxidative leach solution. The results revealed that the precipitation of lithium as lithium carbonate is thermodynamically feasible from the solution at high pHs.
  • Article
    Citation - WoS: 16
    Citation - Scopus: 13
    Production of Mixed Rare Earth Oxide Powder From a Thorium Containing Complex Bastnasite Ore
    (Elsevier, 2021-02) Kursunoglu, Sait; Hussaini, Shokrullah; Top, Soner; Ichlas, Zela Tanlega; Gokcen, Hasan Serkan; Ozsarac, Safak; Kaya, Muammer
    The production of mixed rare earth oxide powder from a thorium containing bastnasite ore by sulfuric acid bake water leaching followed by precipitation with oxalic acid and thermal decomposition of the oxalates was investigated. The sulfuric acid baking was performed at 250 degrees C and the optimum baking time was found to be 3 h. Using deionized water as lixiviant, 92.6% La, 86.8% Ce, 86.9% Pr, 82.3% Nd, 95.4% Th and 31% Y were dissolved from the baked ore at 25 degrees C after 30 min of leaching. The effect of solid-to-liquid ratio on the dissolution of the rare earth elements and thorium shows that when the solid ratio in the water increased from 1:10 to 1:3, the dissolution percentage decreased. The final mixed rare earth oxide powder contained 88.54% REO and 6% ThO20 together with small amounts of other impurities. The SEM mapping results revealed that the produced REO has an irregular crystal shape. Based on the experimental results obtained from the current study, a flowsheet was proposed for the production of mixed rare earth oxide powder from a specific complex bastnasite ore. (C) 2020 Elsevier B.V. All rights reserved.
  • Article
    Citation - WoS: 3
    Citation - Scopus: 3
    A Review on the Recovery of High-Grade Critical Metals From Spent Petroleum Catalysts for Meeting the Demands of Industry 5.0
    (Taylor & Francis inc, 2024-03-22) Taz, Dilara; Ozsarac, Safak; Kursunoglu, Sait; Kursunoglu, Nilufer; Top, Soner; Altiner, Mahmut
    In solvent extraction studies, various extractants, including TOPO, Alamine 308, TBP, TOA, LIX 84I, LIX 63, and Aliquat 336, were employed for the extraction and separation of vanadium, molybdenum, and cobalt from aqueous solutions of spent petroleum catalysts. Results indicated efficient metal recovery using these extractants. Furthermore, a combination of techniques, such as roasting, chemical or bioleaching, solvent extraction (SX), and precipitation, exhibited promising results in achieving comprehensive metal extraction and separation. Important discoveries have been made in the study of recovering important metals from wasted petroleum catalysts, especially with regard to attaining high metal recovery efficiencies. It is found that the recovery efficiency for manganese is 85%, cobalt is 87%, and nickel is 93%. Furthermore, it shows that this procedure may be carried out with high efficiency, with vanadium recovery surpassing 90% and molybdenum recovery efficiency above 95%. These outcomes signify a significant advancement in the field of metal extraction and separation, aligning with the principles of Industry 5.0 while emphasizing sustainability and efficiency in the production of high-tech materials for the modern era.