TR-Dizin İndeksli Yayınlar Koleksiyonu

Permanent URI for this collectionhttps://hdl.handle.net/20.500.12573/396

Browse

Search Results

Now showing 1 - 2 of 2
  • Article
    Citation - Scopus: 2
    Zeolite Synthesis by Alkali Fusion Method Using Two Different Fly Ashes Derived From Turkish Thermal Power Plants
    (Chamber of Mining Engineers of Turkey, 2020-03-01) Top, S.; Vapur, Hüseyin
    In this study, Faujasite (Na-LSX) (3.5(Ca0.3)3.5(Na0.6)3.5(Mg0.1)Al7Si17O48 32(H2O)) type zeolites and Ca-Filipsite (CaK0.6Na0.4Si5.2Al2.8O16 6(H2O)) type zeolites were produced from Sugözü Thermal Power Plant and Çatalaǧzi Thermal Power Plant fly ashes by alkali fusion method followed by water leaching, respectively. In these methods, fly ashes and sodium hydroxide (NaOH) were mixed in certain proportions and sintered at 600°C in ash furnace. Then, zeolites were obtained from the ground materials after water leaching and solid/liquid separation, respectively. Cation Exchange Capacity (CEC), X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Fourier-Transform Infrared Spectroscopy (FTIR), X-Ray Fluorescence (XRF) and Atomic Absorption Spectrometer (AAS) analyses were used to characterize the synthesized zeolites. The zeolites synthesized with Sugözü fly ashes in a ratio of 1:2 had 136.93 meq/100 g CEC, whereas the CEC of synthesized zeolite from Çatalaǧzi fly ashes was found to be 247.88 meq/100 g. As a result, zeolites, which can be used as wastewater treatment agent, energy storage material, catalyst and separator, were synthesized by using 2 different Class F fly ash. © 2023 Elsevier B.V., All rights reserved.
  • Article
    Manganzı Demir Cevherinden Manganın Çözündürülmesinde Farklı İndirgeme Maddelerinin Etkisi
    (Chamber of Mining Engineers of Turkey, 2022-06-26) Top, S.; Altiner, Mahmut; Kursunoglu, Sait
    IIn this paper, the manganese extraction from a manganiferous iron ore was investigated using reductive leaching. Various chemicals were used as a reducing agent to leach manganese selectively from the ore in the presence of sulfuric acid (H2SO4) solution. Firstly, optimum dissolution values were determined for selective manganese dissolution without using a reducing agent. As it was aimed at the selective extraction of manganese from the ore, the reductive leaching tests were conducted by adding the reducing agents under the following optimal parameters: a leaching time of 1 h, a stirring speed of 300 rpm, a temperature of 70°C, a sulfuric acid concentration of 1 M where the ore was leached with an extraction ratio of 11.54% Mn and 2.16% Fe. Manganese was dissolved with high efficiencies (up to 97.46%) from the ore by using different organic compounds (tartaric acid (C<inf>4</inf>H<inf>6</inf>O<inf>6</inf>), oxalic acid (C<inf>2</inf>H<inf>2</inf>O<inf>4</inf>), citric acid (C<inf>6</inf>H<inf>8</inf>O<inf>7</inf>), glucose (C<inf>6</inf>H<inf>12</inf>O<inf>6</inf>), sucrose (C<inf>12</inf>H<inf>22</inf>O<inf>11</inf>), and maleic acid (C<inf>4</inf>H<inf>4</inf>O<inf>4</inf>)) as the reducing agents. © 2022 Elsevier B.V., All rights reserved.